Study of milling time impact on hydrogen desorption from LiAlH4-Fe2O3 composites

Thumbnail
2022
Preuzimanje 🢃
Main article [PDF] (2.133Mb)
Autori
Milanović, Igor
Milošević Govedarović, Sanja S.
Lukić, Miodrag
Jovanović, Zoran
Rmuš, Jelena
Mitrović-Rajić, Anđela
Grbović-Novaković, Jasmina
Kurko, Sandra V.
Članak u časopisu (Objavljena verzija)
Metapodaci
Prikaz svih podataka o dokumentu
Apstrakt
LiAlH4 was modified by mechanical milling and with the addition of 5 wt.% Fe2O3 in order to improve its hydrogen desorption properties. The composite was milled for 1, 3, 5, 7 or 15min, and depending on the milling time, various phenomena took place. Up to a milling time of 5min, the particle size of the composite decreases. Further milling leads to the particles agglomeration reaching the size of the starting material after 15min. Moreover, the mechanical milling process leads to the transformation of AlH - 4 to AlH 3 - 6 structure as a result of partial hydrogen desorption. Hydrogen desorption during the milling is the most pronounced in the sample milled for 15min, so this sample has only one hydrogen desorption peak in the temperature-programmed desorption measurements.Mechanical milling with the addition of Fe2O3 for up to 15min improves LiAlH4 hydrogen desorption properties as hydrogen desorption temperature and apparent activation energies decrease.
Ključne reči:
hydrides / composites / mechanochemical synthesis / hydrogen storage / kinetics
Izvor:
Processing and Application of Ceramics, 2022, 16, 3, 259-266
Finansiranje / projekti:
  • Ministry of Education, Science and Technology of the Republic of Serbia

DOI: 10.2298/PAC2203259M

ISSN: 1820-6131

WoS: 000874799500003

Scopus: 2-s2.0-85141338721
[ Google Scholar ]
2
2
URI
https://vinar.vin.bg.ac.rs/handle/123456789/10504
Kolekcije
  • CEXTREME LAB
  • Radovi istraživača
Institucija/grupa
Vinča
TY  - JOUR
AU  - Milanović, Igor
AU  - Milošević Govedarović, Sanja S.
AU  - Lukić, Miodrag
AU  - Jovanović, Zoran
AU  - Rmuš, Jelena
AU  - Mitrović-Rajić, Anđela
AU  - Grbović-Novaković, Jasmina
AU  - Kurko, Sandra V.
PY  - 2022
UR  - https://vinar.vin.bg.ac.rs/handle/123456789/10504
AB  - LiAlH4 was modified by mechanical milling and with the addition of 5 wt.% Fe2O3 in order to improve its hydrogen desorption properties. The composite was milled for 1, 3, 5, 7 or 15min, and depending on the milling time, various phenomena took place. Up to a milling time of 5min, the particle size of the composite decreases. Further milling leads to the particles agglomeration reaching the size of the starting material after 15min. Moreover, the mechanical milling process leads to the transformation of AlH - 4 to AlH 3 - 6 structure as a result of partial hydrogen desorption. Hydrogen desorption during the milling is the most pronounced in the sample milled for 15min, so this sample has only one hydrogen desorption peak in the temperature-programmed desorption measurements.Mechanical milling with the addition of Fe2O3 for up to 15min improves LiAlH4 hydrogen desorption properties as hydrogen desorption temperature and apparent activation energies decrease.
T2  - Processing and Application of Ceramics
T1  - Study of milling time impact on hydrogen desorption from LiAlH4-Fe2O3 composites
VL  - 16
IS  - 3
SP  - 259
EP  - 266
DO  - 10.2298/PAC2203259M
ER  - 
@article{
author = "Milanović, Igor and Milošević Govedarović, Sanja S. and Lukić, Miodrag and Jovanović, Zoran and Rmuš, Jelena and Mitrović-Rajić, Anđela and Grbović-Novaković, Jasmina and Kurko, Sandra V.",
year = "2022",
abstract = "LiAlH4 was modified by mechanical milling and with the addition of 5 wt.% Fe2O3 in order to improve its hydrogen desorption properties. The composite was milled for 1, 3, 5, 7 or 15min, and depending on the milling time, various phenomena took place. Up to a milling time of 5min, the particle size of the composite decreases. Further milling leads to the particles agglomeration reaching the size of the starting material after 15min. Moreover, the mechanical milling process leads to the transformation of AlH - 4 to AlH 3 - 6 structure as a result of partial hydrogen desorption. Hydrogen desorption during the milling is the most pronounced in the sample milled for 15min, so this sample has only one hydrogen desorption peak in the temperature-programmed desorption measurements.Mechanical milling with the addition of Fe2O3 for up to 15min improves LiAlH4 hydrogen desorption properties as hydrogen desorption temperature and apparent activation energies decrease.",
journal = "Processing and Application of Ceramics",
title = "Study of milling time impact on hydrogen desorption from LiAlH4-Fe2O3 composites",
volume = "16",
number = "3",
pages = "259-266",
doi = "10.2298/PAC2203259M"
}
Milanović, I., Milošević Govedarović, S. S., Lukić, M., Jovanović, Z., Rmuš, J., Mitrović-Rajić, A., Grbović-Novaković, J.,& Kurko, S. V.. (2022). Study of milling time impact on hydrogen desorption from LiAlH4-Fe2O3 composites. in Processing and Application of Ceramics, 16(3), 259-266.
https://doi.org/10.2298/PAC2203259M
Milanović I, Milošević Govedarović SS, Lukić M, Jovanović Z, Rmuš J, Mitrović-Rajić A, Grbović-Novaković J, Kurko SV. Study of milling time impact on hydrogen desorption from LiAlH4-Fe2O3 composites. in Processing and Application of Ceramics. 2022;16(3):259-266.
doi:10.2298/PAC2203259M .
Milanović, Igor, Milošević Govedarović, Sanja S., Lukić, Miodrag, Jovanović, Zoran, Rmuš, Jelena, Mitrović-Rajić, Anđela, Grbović-Novaković, Jasmina, Kurko, Sandra V., "Study of milling time impact on hydrogen desorption from LiAlH4-Fe2O3 composites" in Processing and Application of Ceramics, 16, no. 3 (2022):259-266,
https://doi.org/10.2298/PAC2203259M . .

DSpace software copyright © 2002-2015  DuraSpace
O repozitorijumu VinaR | Pošaljite zapažanja

re3dataOpenAIRERCUB
 

 

Kompletan repozitorijumGrupeAutoriNasloviTemeOva institucijaAutoriNasloviTeme

Statistika

Pregled statistika

DSpace software copyright © 2002-2015  DuraSpace
O repozitorijumu VinaR | Pošaljite zapažanja

re3dataOpenAIRERCUB