dc.description.abstractThe behavior of 16Cr3Al ODS steel (oxide dispersion strengthened steel), widely employed structural fusion material, under high-intensity laser radiation with intensity up to 10(14)W/cm(2) was investigated in air, helium and vacuum surrounding. Employed system was 65 fs laser at 804 nm, with applied pulse energy up to 5.25 mJ. Morphological effects were studied - cracking, crater parameters (depth, cross-section), LIPSS (laser-induced periodic surface structures) formation at the crater periphery, hydrodynamic effects, as well as chemical variations on the surface. Ablation thresholds were also determined for all three ambiences (for 100 applied pulses), and they were 0.30 J/cm(2), 0.23 J/cm(2) and 0.39 J/cm(2) in air, helium and vacuum, respectively. Plasma occurred in all experiments and it was most prominent in vacuum due to strongest laser-material coupling.en
dc.language.isoen
dc.relationinfo:eu-repo/grantAgreement/MESTD/Basic Research (BR or ON)/172019/RS//
dc.relationIAEA Pathways to energy from inertial fusion: Materials beyond ignition [CRP project F13016]
dc.relationEuropean Structural and Investment Funds and the Czech Republic, the project Center of Advanced Applied Science [CZ.02.1.01/0.0/0.0/16_019/0000778] - through The Operational Programme Research, Development and Education
dc.relationCzech Ministry of Education, Youth and Sports [project LTT17015]
dc.rightsrestrictedAccess
dc.sourceFusion Engineering and Design
dc.subjectODS steelen
dc.subjectNuclear materialen
dc.subjectFemtosecond laser surface modificationen
dc.subjectLaser-induced damages/cratersen
dc.subject10(14) W/cm(2) laser intensityen
dc.titleSurface behavior of 16Cr3Al ODS steel—Effects of high laser intensity 1014 W/cm2 in ambiences of air, helium and vacuumen
dc.typearticleen
dc.rights.licenseARR
dcterms.abstractЦигановић, Ј; Сташић, Јелена М.; Тртица, М; Лимпоуцх, Ј; Гаврилов, П; Цхен, X;
dc.rights.holder© 2019 Elsevier B.V.
dc.citation.volume150
dc.citation.spage111360
dc.identifier.wos000504046900024
dc.identifier.doi10.1016/j.fusengdes.2019.111360
dc.citation.rankM21
dc.type.versionpublishedVersion
dc.identifier.scopus2-s2.0-85073821903


Документи

Thumbnail

Овај документ се појављује у следећим колекцијама

Приказ основних података о документу