dc.description.abstractBismuth titanate, Bi4Ti3O12 powders were prepared by mechanically assisted synthesis from their oxides. The diameter of obtained particles depends on time of milling. In order to understand the grain size effects on the crystal structure we measured X-ray, TEM analysis and Raman spectra. The effect of mechanical treatment on the grain size is quite evident: as the milling time increases (3, 6, 12 h), the powder becomes more activated and grain size decrease (7.3, 7.2, 6.9 nm). With reducing the grain size, quantum effects at the Raman spectra, is reflected in the mode position change against balk crystal. And also, coagulation of each line appears, as well as a significant asymmetry of certain modes. (c) 2006 Elsevier B.V. All rights reserved.en
dc.rightsrestrictedAccessen
dc.sourceJournal of Alloys and Compoundsen
dc.subjectmechanochemical synthesisen
dc.subjectcrystal structure and symmetryen
dc.subjectx-ray diffractionen
dc.subjectlight absorption and reflectionen
dc.titleSpectroscopy study of Bi4Ti3O12 obtained from mechanically activated Bi2O3-TiO2 mixturesen
dc.typearticleen
dcterms.abstractЛазаревиц, З.; Ромцевиц, М.; Јовалекиц, Ц.; Ромцевиц, Н.; Стојановиц, Б.; Митрић Миодраг;
dc.citation.volume453
dc.citation.issue1-2
dc.citation.spage499
dc.citation.epage502
dc.identifier.wos000254899700091
dc.identifier.doi10.1016/j.jailcom.2006.11.198
dc.citation.rankM21


Документи

ДатотекеВеличинаФорматПреглед

Уз овај запис нема датотека.

Овај документ се појављује у следећим колекцијама

Приказ основних података о документу