Претраживање
Приказ резултата 1-2 од 2
Synthesis of Barium-zinc-titanate Ceramics
(Science of Sintering, 2012)
Mixtures of BaCO3, ZnO and TiO2 powders, with molar ratio of 1:2:4, were mechanically activated for 20, 40 and minutes in a planetary ball mill. The resulting powders were compacted into pellets and isothermally sintered ...
Influence of Mechanical Activation on Microstructure and Crystal Structure of Sintered MgO-TiO2 System
(Science of Sintering, 2010)
Mixtures of MgO-TiO2 were mechanically activated using high-energy planetary ball mill during 5, 10, 20, 40, 80 and 120 minutes. Sintering process was preformed in air at 1100 degrees-1400 degrees C for 2h. The decrease ...