Influence of MgO addition on the synthesis and electrical properties of sintered zinc-titanate ceramics
(Journal of Alloys and Compounds, 2009)
Starting mixtures of ZnO, TiO(2) and MgO (0, 1.25 and 2.5 wt.% MgO) powders were mechanically activated for 15 min in a planetary ball mill. The powders obtained were sintered non-isothermally to temperatures between 800 ...
Synthesis of Barium-zinc-titanate Ceramics
(Science of Sintering, 2012)
Mixtures of BaCO3, ZnO and TiO2 powders, with molar ratio of 1:2:4, were mechanically activated for 20, 40 and minutes in a planetary ball mill. The resulting powders were compacted into pellets and isothermally sintered ...
Influence of Mechanical Activation on Microstructure and Crystal Structure of Sintered MgO-TiO2 System
(Science of Sintering, 2010)
Mixtures of MgO-TiO2 were mechanically activated using high-energy planetary ball mill during 5, 10, 20, 40, 80 and 120 minutes. Sintering process was preformed in air at 1100 degrees-1400 degrees C for 2h. The decrease ...