Effect of LiYO(2) addition on sintering behavior and indentation properties of silicon nitride ceramics

Matović, Branko; Rixecker, Georg; Bošković, Snežana B.; Aldinger, Fritz

(2006)

TY  - JOUR
AU  - Matović, Branko
AU  - Rixecker, Georg
AU  - Bošković, Snežana B.
AU  - Aldinger, Fritz
PY  - 2006
UR  - https://vinar.vin.bg.ac.rs/handle/123456789/3104
AB  - The influence of the sintering additive LiYO(2) (5-15 wt.%) on sintering behavior, microstructure and mechanical properties of Si(3)N(4) ceramics was investigated. Since LiYO(2) enables densification of Si(3)N(4) at extraordinarily low temperatures, sintering was carried out in the range from 1200-1700 degrees C. Densification was found to be enhanced with increasing additive content due to an increasing volume fraction of the liquid. The phase transformation and grain growth occurred through a solution-reprecipitation mechanism, where the precipitation took place preferentially on pre-existing beta-Si(3)N(4) nuclei (of which the starting powder already contained 20 wt.%). The indentation fracture toughness increased with both sintering time and additive content as a result of the growth of elongated grains.
T2  - International Journal of Materials Research
T1  - Effect of LiYO(2) addition on sintering behavior and indentation properties of silicon nitride ceramics
VL  - 97
IS  - 9
SP  - 1268
EP  - 1272
DO  - 10.3139/146.101368
ER  - 
@article{
author = "Matović, Branko and Rixecker, Georg and Bošković, Snežana B. and Aldinger, Fritz",
year = "2006",
abstract = "The influence of the sintering additive LiYO(2) (5-15 wt.%) on sintering behavior, microstructure and mechanical properties of Si(3)N(4) ceramics was investigated. Since LiYO(2) enables densification of Si(3)N(4) at extraordinarily low temperatures, sintering was carried out in the range from 1200-1700 degrees C. Densification was found to be enhanced with increasing additive content due to an increasing volume fraction of the liquid. The phase transformation and grain growth occurred through a solution-reprecipitation mechanism, where the precipitation took place preferentially on pre-existing beta-Si(3)N(4) nuclei (of which the starting powder already contained 20 wt.%). The indentation fracture toughness increased with both sintering time and additive content as a result of the growth of elongated grains.",
journal = "International Journal of Materials Research",
title = "Effect of LiYO(2) addition on sintering behavior and indentation properties of silicon nitride ceramics",
volume = "97",
number = "9",
pages = "1268-1272",
doi = "10.3139/146.101368"
}
Matović, B., Rixecker, G., Bošković, S. B.,& Aldinger, F.. (2006). Effect of LiYO(2) addition on sintering behavior and indentation properties of silicon nitride ceramics. in International Journal of Materials Research, 97(9), 1268-1272.
https://doi.org/10.3139/146.101368
Matović B, Rixecker G, Bošković SB, Aldinger F. Effect of LiYO(2) addition on sintering behavior and indentation properties of silicon nitride ceramics. in International Journal of Materials Research. 2006;97(9):1268-1272.
doi:10.3139/146.101368 .
Matović, Branko, Rixecker, Georg, Bošković, Snežana B., Aldinger, Fritz, "Effect of LiYO(2) addition on sintering behavior and indentation properties of silicon nitride ceramics" in International Journal of Materials Research, 97, no. 9 (2006):1268-1272,
https://doi.org/10.3139/146.101368 . .