@article{
author = "Vilotijević, Miroljub N. and Markovic, Petar and Zec, Slavica and Marinković, Slobodan N. and Jokanović, Vukoman R.",
year = "2011",
abstract = "For two hydroxyapatite (HA) powders, containing particles differing in mass by a factor of 20, a set of optimum deposition parameters was defined, leading to the coatings with high crystallinity (80-90%), high adhesion strength (60 and 40 MPa for the coating thicknesses of 120 mu m and 350 mu m, respectively) and excellent microstructure (coatings were without micro- or macro-cracks, without delaminating on substrate-coating surface contact, and possess low porosity, 1-2%). It was shown that higher plasma power (52 kW) did not necessarily lead to a higher HA decomposition. (C) 2011 Elsevier B.V. All rights reserved.",
journal = "Journal of Materials Processing Technology",
title = "Hydroxyapatite coatings prepared by a high power laminar plasma jet",
volume = "211",
number = "6",
pages = "996-1004",
doi = "10.1016/j.jmatprotec.2010.12.018"
}