Gubeljak, Nenad

Link to this page

Authority KeyName Variants
orcid::0000-0002-3276-8431
  • Gubeljak, Nenad (1)
Projects

Author's Bibliography

Microstructure, hardness and fracture resistance of P235TR1 seam steel pipes of different diameters

Musrati, Walid; Međo, Bojan; Cvijović-Alagić, Ivana; Gubeljak, Nenad; Štefane, Primož; Radosavljević, Zoran; Rakin, Marko

(2023)

TY  - JOUR
AU  - Musrati, Walid
AU  - Međo, Bojan
AU  - Cvijović-Alagić, Ivana
AU  - Gubeljak, Nenad
AU  - Štefane, Primož
AU  - Radosavljević, Zoran
AU  - Rakin, Marko
PY  - 2023
UR  - https://vinar.vin.bg.ac.rs/handle/123456789/11325
AB  - Steel pipelines in industrial plants consist of different elements, including seamless and/or welded (seam) pipes. Properties of welded pipes, including their fracture behaviour, depend on the characteristics of both, the base metal, and the weld metal. In this work, two seam pipes are considered having different diameters and manufactured of P235TR1 steel. Hardness and microstructure were examined on the samples which contained the seam zone, to capture the influence of heterogeneity. Fracture resistance of the pipeline material, i.e. of both base metals and both seams, was determined by experimental examination of the recently proposed Pipe ring notch bending specimens with sharp stress concentrators. Differences between the two tested pipes, including the influence of the heterogeneity caused by the welded joint, were determined by comparison of the crack growth resistance curves. Effects of the initial stress concentrator shape, sharp machined notch or fatigue pre-crack are discussed.
AB  - Čelični cevovodi u industrijskim postrojenjima se sastoje od različitih elemenata, uključujući bešavne i/ili zavarene (šavne) cevi. Osobine šavnih cevi, uključujući ponašanje materijala cevi pri lomu, zavise i od osnovnog metala i od metala šava. U ovom radu razmatrane su dve šavne cevi različitih prečnika, izrađene od čelika P235TR1. Tvrdoća i mikrostruktura su analizirane na uzorcima isečenim iz cevi u zoni šava, da bi se odredio uticaj heterogenosti. Otpornost prema lomu materijala cevovoda, tj. oba osnovna metala i oba šava, je određena na osnovu ispitivanja epruveta oblika prstena sa oštrim koncentratorima napona, predloženih u prethodnim studijama. Poređenjem krivih otpornosti prema rastu prsline određene su razlike između dve ispitivane cevi, kao i uticaj heterogenosti izazvan postojanjem zavarenog spoja. Razmotren je uticaj oblika početnog koncentratora napona, oštrog žleba odnosno zamorne početne prsline.
T2  - Hemijska industrija
T1  - Microstructure, hardness and fracture resistance of P235TR1 seam steel pipes of different diameters
T1  - Otpornost prema lomu, tvrdoća i mikrostruktura šavnih cevi različitog prečnika izrađenih od čelika P235TR1
VL  - 77
IS  - 2
SP  - 155
EP  - 165
DO  - 10.2298/HEMIND230222016M
ER  - 
@article{
author = "Musrati, Walid and Međo, Bojan and Cvijović-Alagić, Ivana and Gubeljak, Nenad and Štefane, Primož and Radosavljević, Zoran and Rakin, Marko",
year = "2023",
abstract = "Steel pipelines in industrial plants consist of different elements, including seamless and/or welded (seam) pipes. Properties of welded pipes, including their fracture behaviour, depend on the characteristics of both, the base metal, and the weld metal. In this work, two seam pipes are considered having different diameters and manufactured of P235TR1 steel. Hardness and microstructure were examined on the samples which contained the seam zone, to capture the influence of heterogeneity. Fracture resistance of the pipeline material, i.e. of both base metals and both seams, was determined by experimental examination of the recently proposed Pipe ring notch bending specimens with sharp stress concentrators. Differences between the two tested pipes, including the influence of the heterogeneity caused by the welded joint, were determined by comparison of the crack growth resistance curves. Effects of the initial stress concentrator shape, sharp machined notch or fatigue pre-crack are discussed., Čelični cevovodi u industrijskim postrojenjima se sastoje od različitih elemenata, uključujući bešavne i/ili zavarene (šavne) cevi. Osobine šavnih cevi, uključujući ponašanje materijala cevi pri lomu, zavise i od osnovnog metala i od metala šava. U ovom radu razmatrane su dve šavne cevi različitih prečnika, izrađene od čelika P235TR1. Tvrdoća i mikrostruktura su analizirane na uzorcima isečenim iz cevi u zoni šava, da bi se odredio uticaj heterogenosti. Otpornost prema lomu materijala cevovoda, tj. oba osnovna metala i oba šava, je određena na osnovu ispitivanja epruveta oblika prstena sa oštrim koncentratorima napona, predloženih u prethodnim studijama. Poređenjem krivih otpornosti prema rastu prsline određene su razlike između dve ispitivane cevi, kao i uticaj heterogenosti izazvan postojanjem zavarenog spoja. Razmotren je uticaj oblika početnog koncentratora napona, oštrog žleba odnosno zamorne početne prsline.",
journal = "Hemijska industrija",
title = "Microstructure, hardness and fracture resistance of P235TR1 seam steel pipes of different diameters, Otpornost prema lomu, tvrdoća i mikrostruktura šavnih cevi različitog prečnika izrađenih od čelika P235TR1",
volume = "77",
number = "2",
pages = "155-165",
doi = "10.2298/HEMIND230222016M"
}
Musrati, W., Međo, B., Cvijović-Alagić, I., Gubeljak, N., Štefane, P., Radosavljević, Z.,& Rakin, M.. (2023). Microstructure, hardness and fracture resistance of P235TR1 seam steel pipes of different diameters. in Hemijska industrija, 77(2), 155-165.
https://doi.org/10.2298/HEMIND230222016M
Musrati W, Međo B, Cvijović-Alagić I, Gubeljak N, Štefane P, Radosavljević Z, Rakin M. Microstructure, hardness and fracture resistance of P235TR1 seam steel pipes of different diameters. in Hemijska industrija. 2023;77(2):155-165.
doi:10.2298/HEMIND230222016M .
Musrati, Walid, Međo, Bojan, Cvijović-Alagić, Ivana, Gubeljak, Nenad, Štefane, Primož, Radosavljević, Zoran, Rakin, Marko, "Microstructure, hardness and fracture resistance of P235TR1 seam steel pipes of different diameters" in Hemijska industrija, 77, no. 2 (2023):155-165,
https://doi.org/10.2298/HEMIND230222016M . .