PVDF-HFP/NKBT composite dielectrics: Perovskite particles induce the appearance of an additional dielectric relaxation process in ferroelectric polymer matrix
Autori
Pavlović, Vera P.Tošić, Dragana
Dojčilović, Radovan
Dudić, Duško
Dramićanin, Miroslav
Medić, Mina M.
McPherson, Michael M.
Pavlović, Vladimir B.
Vlahović, Branislav
Đoković, Vladimir
Članak u časopisu (Objavljena verzija)
Metapodaci
Prikaz svih podataka o dokumentuApstrakt
Na0.25K0.25Bi0.5TiO3 (NKBT) perovskite particles are synthesized by solid-state method and used as a filler for polyvinylidene fluoride-co-hexafluoropropylene (PVDF-HFP) co-polymer. X-ray diffraction analysis of NKBT powders shows that the particles have a rhombohedral perovskite crystal structure (R3c symmetry). Raman spectroscopy reveals that the co-polymer crystallizes predominantly into the mixture of polar β- and γ-crystals, while there is also a contribution of the non-polar α-crystal phase. The introduction of the NKBT into the PVDF-HFP results with an increase in effective dielectric permittivity and this effect depends on the inorganic content in the composite. The most interesting result of the present study is that the introduction of NKBT particles induces the appearance of an additional transition peak in the dielectric spectra of the co-polymer matrix. At the fixed frequency of ~2 kHz, the observed process appears at ~10 °C (about 45° above the glass transition temperatur...e) and its magnitude strongly depends on the amount of the NKBT in the composite. Dielectric spectroscopy measurements of the composites are carried out in the wide range of frequencies (from 0.1 Hz to 1 MHz) and temperatures (from −100 to 100 °C). They reveal that the novel process can be clearly distinguished in the frequency range between 160 Hz and ~50 kHz. © 2021 The Authors
Ključne reči:
Dielectric relaxation spectroscopy / PVDF-HFP / Composite / Perovskite / NKBTIzvor:
Polymer Testing, 2021, 96, 107093-Finansiranje / projekti:
- Uticaj veličine, oblika i strukture nanočestica na njihova svojstva i svojstva nanokompozita (RS-MESTD-Basic Research (BR or ON)-172056)
- Materijali redukovane dimenzionalnosti za efikasnu apsorpciju svetlosti i konverziju energije (RS-MESTD-Integrated and Interdisciplinary Research (IIR or III)-45020)
- Proučavanje uticaja tretiranja na dielektrične, optičke, magnetne i osobine površina kristalnih i polimernih sistema (RS-MESTD-Basic Research (BR or ON)-171029)
- NSF CREST [HRD-0833184]
- NSF [1523617]
DOI: 10.1016/j.polymertesting.2021.107093
ISSN: 0142-9418
WoS: 000663792300029
Scopus: 2-s2.0-85100677797
Kolekcije
Institucija/grupa
VinčaTY - JOUR AU - Pavlović, Vera P. AU - Tošić, Dragana AU - Dojčilović, Radovan AU - Dudić, Duško AU - Dramićanin, Miroslav AU - Medić, Mina M. AU - McPherson, Michael M. AU - Pavlović, Vladimir B. AU - Vlahović, Branislav AU - Đoković, Vladimir PY - 2021 UR - https://vinar.vin.bg.ac.rs/handle/123456789/9563 AB - Na0.25K0.25Bi0.5TiO3 (NKBT) perovskite particles are synthesized by solid-state method and used as a filler for polyvinylidene fluoride-co-hexafluoropropylene (PVDF-HFP) co-polymer. X-ray diffraction analysis of NKBT powders shows that the particles have a rhombohedral perovskite crystal structure (R3c symmetry). Raman spectroscopy reveals that the co-polymer crystallizes predominantly into the mixture of polar β- and γ-crystals, while there is also a contribution of the non-polar α-crystal phase. The introduction of the NKBT into the PVDF-HFP results with an increase in effective dielectric permittivity and this effect depends on the inorganic content in the composite. The most interesting result of the present study is that the introduction of NKBT particles induces the appearance of an additional transition peak in the dielectric spectra of the co-polymer matrix. At the fixed frequency of ~2 kHz, the observed process appears at ~10 °C (about 45° above the glass transition temperature) and its magnitude strongly depends on the amount of the NKBT in the composite. Dielectric spectroscopy measurements of the composites are carried out in the wide range of frequencies (from 0.1 Hz to 1 MHz) and temperatures (from −100 to 100 °C). They reveal that the novel process can be clearly distinguished in the frequency range between 160 Hz and ~50 kHz. © 2021 The Authors T2 - Polymer Testing T1 - PVDF-HFP/NKBT composite dielectrics: Perovskite particles induce the appearance of an additional dielectric relaxation process in ferroelectric polymer matrix VL - 96 SP - 107093 DO - 10.1016/j.polymertesting.2021.107093 ER -
@article{ author = "Pavlović, Vera P. and Tošić, Dragana and Dojčilović, Radovan and Dudić, Duško and Dramićanin, Miroslav and Medić, Mina M. and McPherson, Michael M. and Pavlović, Vladimir B. and Vlahović, Branislav and Đoković, Vladimir", year = "2021", abstract = "Na0.25K0.25Bi0.5TiO3 (NKBT) perovskite particles are synthesized by solid-state method and used as a filler for polyvinylidene fluoride-co-hexafluoropropylene (PVDF-HFP) co-polymer. X-ray diffraction analysis of NKBT powders shows that the particles have a rhombohedral perovskite crystal structure (R3c symmetry). Raman spectroscopy reveals that the co-polymer crystallizes predominantly into the mixture of polar β- and γ-crystals, while there is also a contribution of the non-polar α-crystal phase. The introduction of the NKBT into the PVDF-HFP results with an increase in effective dielectric permittivity and this effect depends on the inorganic content in the composite. The most interesting result of the present study is that the introduction of NKBT particles induces the appearance of an additional transition peak in the dielectric spectra of the co-polymer matrix. At the fixed frequency of ~2 kHz, the observed process appears at ~10 °C (about 45° above the glass transition temperature) and its magnitude strongly depends on the amount of the NKBT in the composite. Dielectric spectroscopy measurements of the composites are carried out in the wide range of frequencies (from 0.1 Hz to 1 MHz) and temperatures (from −100 to 100 °C). They reveal that the novel process can be clearly distinguished in the frequency range between 160 Hz and ~50 kHz. © 2021 The Authors", journal = "Polymer Testing", title = "PVDF-HFP/NKBT composite dielectrics: Perovskite particles induce the appearance of an additional dielectric relaxation process in ferroelectric polymer matrix", volume = "96", pages = "107093", doi = "10.1016/j.polymertesting.2021.107093" }
Pavlović, V. P., Tošić, D., Dojčilović, R., Dudić, D., Dramićanin, M., Medić, M. M., McPherson, M. M., Pavlović, V. B., Vlahović, B.,& Đoković, V.. (2021). PVDF-HFP/NKBT composite dielectrics: Perovskite particles induce the appearance of an additional dielectric relaxation process in ferroelectric polymer matrix. in Polymer Testing, 96, 107093. https://doi.org/10.1016/j.polymertesting.2021.107093
Pavlović VP, Tošić D, Dojčilović R, Dudić D, Dramićanin M, Medić MM, McPherson MM, Pavlović VB, Vlahović B, Đoković V. PVDF-HFP/NKBT composite dielectrics: Perovskite particles induce the appearance of an additional dielectric relaxation process in ferroelectric polymer matrix. in Polymer Testing. 2021;96:107093. doi:10.1016/j.polymertesting.2021.107093 .
Pavlović, Vera P., Tošić, Dragana, Dojčilović, Radovan, Dudić, Duško, Dramićanin, Miroslav, Medić, Mina M., McPherson, Michael M., Pavlović, Vladimir B., Vlahović, Branislav, Đoković, Vladimir, "PVDF-HFP/NKBT composite dielectrics: Perovskite particles induce the appearance of an additional dielectric relaxation process in ferroelectric polymer matrix" in Polymer Testing, 96 (2021):107093, https://doi.org/10.1016/j.polymertesting.2021.107093 . .