dc.description.abstractA subsecond pulse heating method was applied to measure the specific heat capacity, electrical resistivity, total hemispherical emissivity, and normal spectral emissivity of 99.9% pure tantalum in the form of 2-mm-diameter wire. W/Re thermocouple thermometry was applied from 300 to 2300 K, with emissivity measurements above 1300 K involving pyrometric measurements. The maximum uncertainties in the specific heat capacity and electrical resistivity were less than 3 and 1% respectively. The uncertainty of emissivity measurements was estimated as +/- 5 %. The results are compared with literature values.en
dc.rightsrestrictedAccessen
dc.sourceInternational Journal of Thermophysicsen
dc.subjectelectrical conductorsen
dc.subjectelectrical resistivityen
dc.subjecthemispherical total emissivityen
dc.subjecthigh temperaturesen
dc.subjectnormal spectral emissivityen
dc.subjectrefractory metalsen
dc.subjectspecific heaten
dc.subjecttantalumen
dc.titleThermal properties of tantalum between 300 and 2300 Ken
dc.typearticleen
dcterms.abstractПавициц, ДЗ; Милошевић Ненад; Маглиц, КД; Вуковиц, ГС;
dc.citation.volume20
dc.citation.issue4
dc.citation.spage1129
dc.citation.epage1136
dc.identifier.wos000083255400013
dc.identifier.doi10.1023/A:1022659005050
dc.citation.rankM21
dc.description.other5th International Workshop on Subsecond Thermophysics, Jun 16-19, 1998, Aix-En Provence, Franceen
dc.identifier.scopus2-s2.0-0032594764


Документи

ДатотекеВеличинаФорматПреглед

Уз овај запис нема датотека.

Овај документ се појављује у следећим колекцијама

Приказ основних података о документу