dc.creatorRistić, Gordana
dc.creatorPetkovska, Ljubica T.
dc.creatorBogdanov, Žarko
dc.creatorZec, Slavica
dc.creatorMiljanić, Šćepan S.
dc.date.accessioned2018-03-01T14:06:48Z
dc.date.available2018-03-01T14:06:48Z
dc.date.issued1998
dc.identifier.issn0352-5139
dc.identifier.urihttps://vinar.vin.bg.ac.rs/handle/123456789/46
dc.description.abstractA tungsten filament, 0.12 mm in diameter, was conditioned by heating in a mixture of methane and hydrogen of three different concentration ratios. The filament was heated by an electric current. The procedure was carried out stepwise keeping either the voltage or the temperature of the filament constant. Changes in the filament material were monitored by resistance and temperature measurements. The chemical composition was checked using X-ray diffraction (XRD) analysis. The final state of the filament was investigated and photographed using the scanning-electron microscopy (SEM) technique.en
dc.rightsopenAccessen
dc.rights.urihttps://creativecommons.org/licenses/by-nc-nd/4.0/
dc.sourceJournal of the Serbian Chemical Societyen
dc.subjecthot-filamenten
dc.subjectconditioningen
dc.subjectcarburizationen
dc.subjectdiamond depositionen
dc.subjecthfCVDen
dc.titleConditioning of the filament for diamond deposition by hot-filament chemical vapour deposition methoden
dc.typearticleen
dc.rights.licenseBY-NC-ND
dcterms.abstractРистиц, ГС; Богданов Жарко; Миљаниц, СС; Зец Славица; Петковска, ЛТ;
dc.citation.volume63
dc.citation.issue3
dc.citation.spage231
dc.citation.epage235
dc.identifier.wos000072976900009
dc.type.versionpublishedVersion
dc.identifier.rcubhttps://hdl.handle.net/21.15107/rcub_vinar_46


Dokumenti

DatotekeVeličinaFormatPregled

Uz ovaj zapis nema datoteka.

Ovaj dokument se pojavljuje u sledećim kolekcijama

Prikaz osnovnih podataka o dokumentu