Приказ основних података о документу
Metal phosphate preparation using boron phosphate
dc.creator | Vasović, Dušanka D. | |
dc.creator | Stojakovic, Đorđe R. | |
dc.creator | Zec, Slavica | |
dc.date.accessioned | 2018-03-01T18:20:07Z | |
dc.date.available | 2018-03-01T18:20:07Z | |
dc.date.issued | 1997 | |
dc.identifier.issn | 0025-5408 | |
dc.identifier.uri | https://vinar.vin.bg.ac.rs/handle/123456789/2066 | |
dc.description.abstract | The solid-state conversion of basic magnesium, calcium, zinc, and lead compounds into corresponding crystalline phosphates by the BPO4 method has been investigated at 800 degrees C and 900 degrees C. Magnesium hydroxide carbonate is converted at 800 degrees C into Mg2P2O7 (85%), whereas calcium hydroxide gives 2CaO . P2O5 . B2O3 at 900 degrees C. Zinc oxide gives at 800 degrees C the mixture of Zn2P2O7 (90%) and Zn-3(PO4)(2) (10%), whereas at 900 degrees C only the former is obtained. In the presence of KCl, at 800 degrees C, zinc oxide yields KZnPO4, while PbO gives Pb-5(PO4)(3)Cl. (C) 1997 Elsevier Science Ltd. | en |
dc.relation | Research Fund of Serbia | |
dc.rights | restrictedAccess | en |
dc.source | Materials Research Bulletin | en |
dc.subject | inorganic compounds | en |
dc.subject | chemical synthesis | en |
dc.subject | X-ray diffraction | en |
dc.title | Metal phosphate preparation using boron phosphate | en |
dc.type | article | en |
dc.rights.license | ARR | |
dcterms.abstract | Васовиц, ДД; Зец Славица; Стојаковиц, ДР; | |
dc.citation.volume | 32 | |
dc.citation.issue | 6 | |
dc.citation.spage | 779 | |
dc.citation.epage | 784 | |
dc.identifier.wos | A1997XA49400017 | |
dc.identifier.doi | 10.1016/S0025-5408(97)00043-3 | |
dc.type.version | publishedVersion | |
dc.identifier.scopus | 2-s2.0-0031170077 |