Fine agglomerate-free spherical beta-SiC powder was synthesized from a dispersion of colloidal silica, saccharose, and boric acid, by means of an ultrasonic spray pyrolysis method, Droplets of 2.2 mu m were formed with an aerosol generator, operated at 2.5 MHz, and carried into a reaction furnace at 900 degrees C with argon, Spherical X-ray amorphous gel particles of 1.1 mu m were obtained, beta-SiC particles with a mean diameter of 0.79 mu m and spherical shape resulted when the SiC gel precursor particles were heated at 1500 degrees C in argon.
Извор:
Journal of the American Ceramic Society, 1996, 79, 8, 2215-2217
DOI: 10.1111/j.1151-2916.1996.tb08964.x
ISSN: 0002-7820
WoS: A1996VC61300036
Scopus: 2-s2.0-0030214054
Колекције
Институција/група
VinčaTY - JOUR AU - Čerović, Ljiljana S. AU - Milonjić, Slobodan K. AU - Živković, Ljiljana V. AU - Uskoković, Dragan PY - 1996 UR - https://vinar.vin.bg.ac.rs/handle/123456789/2008 AB - Fine agglomerate-free spherical beta-SiC powder was synthesized from a dispersion of colloidal silica, saccharose, and boric acid, by means of an ultrasonic spray pyrolysis method, Droplets of 2.2 mu m were formed with an aerosol generator, operated at 2.5 MHz, and carried into a reaction furnace at 900 degrees C with argon, Spherical X-ray amorphous gel particles of 1.1 mu m were obtained, beta-SiC particles with a mean diameter of 0.79 mu m and spherical shape resulted when the SiC gel precursor particles were heated at 1500 degrees C in argon. T2 - Journal of the American Ceramic Society T1 - Synthesis of spherical beta-silicon carbide particles by ultrasonic spray pyrolysis VL - 79 IS - 8 SP - 2215 EP - 2217 DO - 10.1111/j.1151-2916.1996.tb08964.x ER -
@article{ author = "Čerović, Ljiljana S. and Milonjić, Slobodan K. and Živković, Ljiljana V. and Uskoković, Dragan", year = "1996", abstract = "Fine agglomerate-free spherical beta-SiC powder was synthesized from a dispersion of colloidal silica, saccharose, and boric acid, by means of an ultrasonic spray pyrolysis method, Droplets of 2.2 mu m were formed with an aerosol generator, operated at 2.5 MHz, and carried into a reaction furnace at 900 degrees C with argon, Spherical X-ray amorphous gel particles of 1.1 mu m were obtained, beta-SiC particles with a mean diameter of 0.79 mu m and spherical shape resulted when the SiC gel precursor particles were heated at 1500 degrees C in argon.", journal = "Journal of the American Ceramic Society", title = "Synthesis of spherical beta-silicon carbide particles by ultrasonic spray pyrolysis", volume = "79", number = "8", pages = "2215-2217", doi = "10.1111/j.1151-2916.1996.tb08964.x" }
Čerović, L. S., Milonjić, S. K., Živković, L. V.,& Uskoković, D.. (1996). Synthesis of spherical beta-silicon carbide particles by ultrasonic spray pyrolysis. in Journal of the American Ceramic Society, 79(8), 2215-2217. https://doi.org/10.1111/j.1151-2916.1996.tb08964.x
Čerović LS, Milonjić SK, Živković LV, Uskoković D. Synthesis of spherical beta-silicon carbide particles by ultrasonic spray pyrolysis. in Journal of the American Ceramic Society. 1996;79(8):2215-2217. doi:10.1111/j.1151-2916.1996.tb08964.x .
Čerović, Ljiljana S., Milonjić, Slobodan K., Živković, Ljiljana V., Uskoković, Dragan, "Synthesis of spherical beta-silicon carbide particles by ultrasonic spray pyrolysis" in Journal of the American Ceramic Society, 79, no. 8 (1996):2215-2217, https://doi.org/10.1111/j.1151-2916.1996.tb08964.x . .